CaCo3 Powder
There are two main reasons why CaCO₃ is used in plastic: it acts as a functional filler or mineral modifier (e.g. to produce
breathable films) or it is used to reduce the costs of the compound.
What is important when using CaCO₃ is its very good incorporation in the polymer matrix. Coated CaCO₃ types are the most
suitable because the surface coating adjusts the surface tension of the mineral to that of the polymer, greatly facilitating its
incorporation and dispersion.
1. Advantages of CaCO3 Filler Masterbatch for each application in plastic industries:
Filler masterbatch are used in injection, blow-moulding, film(One layer or Multiple layer), sheet and tapes applications. They offer the following advantages:1.1 Injection & blow-moulding
- Lower raw materials cost, as they are usually more economic than polymer resins
- Increased output due to faster mould cooling
- Reduction of colour masterbatch requirement
- Higher resistance to heat deflection, higher rigidity and stiffness
- Improved dimensional stability, weldability and printability
- Addition rate of Filler masterbatch in injection & blow-moulding applications can be up to 50 %, however, most usual levels are between 5-30 %.
1.2 Film, sheet, sacks, bags, raffia
- Lower raw materials cost, as they are usually more economic than polymer resins
- Reduction of colour masterbatch requirement
- Higher stiffness, paper-like effect
- Improved weldability and printability
- Improved anti-blocking properties
- Better bubble stability
- Addition rate of FILLER masterbatch in film applications is 2-20 %.
1.3 PE & PP tapes
- Antifibrillation (also known as anti splitting)
- Lower raw materials cost, as they are usually more economic than polymer resins
- Reduction of colour masterbatch requirement
- Higher stiffness
- Improved weldability and printability
- Improved anti-blocking properties
- Improved weaving ability
- Easier processing
- Usual addition rate of Filler masterbatchin tapes is 3-8 %.
1.4 HDPE & PP Pipe
- Replacing expensive white masterbatch with its high white degree
- Lower raw materials cost, as they are usually more economic than polymer resins
- Higher stiffness
- Smooth pipes with lower coefficient of friction to better prevent them from blocking
- Being less possible to be brittel in low temperature adue to its excellent cold resistance
- Usual addition rate of Filler masterbatch in tapes is 5-30 %.
2. How to produce Filler Masterbatch?
2.1 Feeding System
- There two feeding system:
- Volumetric feeding system
- Loss-in-weight feeding system (automatically and higher accuracy)
2.2 Technical Specifications of Extruder
- Twin Screw Extruder
- Triple Screw Extruder